Two HDPE supplier sheets both quote 0.955 g/cm3. One reports melt index at 190 °C/2.16 kg; the other at 190 °C/21.6 kg. One gives ESCR as an F50 with reagent and temperature; the other says good. Put either resin in the same ES-10LS and mold, and parison, wall and cycle will not match. Neither number means anything without its test condition.

The short answer: density for stiffness, melt index for flow

Density sets stiffness, shrinkage and ESCR; melt index sets flow and parison sag. Specify both with their test conditions, never as a single rank. A typical blow molding window is 0.95–0.96 g/cm3 and 0.2–0.5 g/10 min at 190 °C/2.16 kg, to be confirmed with the resin supplier.

Density: the number behind stiffness, shrinkage and ESCR

Density is mass per unit volume, and in HDPE it tracks crystallinity. Higher density gives a stiffer bottle, better stack strength and usually better moisture barrier, but lower ESCR. Lower density gives more toughness and ESCR, but less stiffness. A 0.955 grade is not automatically better than 0.950; they answer different requirements.

Two grades can both print 0.955 g/cm3 and still behave differently. Comonomer and molecular weight distribution change melt behaviour and crack resistance. Ask for the test method and lot tolerance.

Shrinkage is where density meets the mold. HDPE is semi-crystalline; datasheets give a shrinkage range, which differs along and across flow with wall thickness. Use the range for first mold dimensions, then confirm on a trial with the production mold.

ESCR is the other density-linked property. It is measured under constant stress in a chemical environment; F50 is the time at which 50% of specimens fail. Without reagent, concentration, temperature, specimen and stress, an F50 cannot be compared with another sheet.

Melt index: never compare without the load

Melt index (MI or MFI) is the mass of polymer flowing through a die in ten minutes at a fixed temperature and load. For polyethylene the temperature is normally 190 °C, but the load may be 2.16 kg, 5 kg or 21.6 kg. The 21.6 kg load is ten times the 2.16 kg load, so the same polymer reports a much larger number; the values do not convert by a simple ratio.

Read MI as a flow signal. Higher MI means lower melt viscosity: the parison flows more easily and the extruder needs less torque, but melt strength falls, so a long parison can sag or swing before the mold closes. Lower MI gives more melt strength for a heavy container, but the extruder works harder.

On a 5 L bottle running on an ES-5LS (60–65 mm screw, 65–80 kg/h), a higher-MI grade can make a thin wall easier to fill, but the die gap and parison programmer still set the wall. On a 10 L container on an ES-10LS (70–75 mm screw, 80–100 kg/h), the longer parison makes melt strength and sag control matter more. Measure the cycle with the actual mold.

For the container side, readHDPE bottle blow molding, and for the 20–50 L route,25 L lubricant oil bottle production. Machine fit is covered by the0.1–16 L single-station rangeand thedouble-station range.

The five-field datasheet check

A datasheet is a comparison document, not a label. Put both suppliers' sheets into the same five fields. If a number has no method or condition, treat it as unconfirmed.

Five fields to compare before a resin trial. Read each value with its method and condition; confirm limits with the resin supplier.
Datasheet field What to read What it controls What to confirm
DensityNominal value, test method, lot toleranceStiffness, stack strength, shrinkage, ESCR trendA grade nominal with a tolerance, not one lab result
Melt indexValue with load and temperature: 2.16, 5 or 21.6 kg at 190 °CFlow, extruder load, parison sagSame condition as your reference, or the raw report
ESCRReagent, concentration, temperature, specimen, F50Service life under the filling productConditions that match your product; otherwise not comparable
Mold shrinkageRange and direction, with wall thicknessMold dimensions, fit and warpageA trial on the production mold before approval
Food-contact status and CoADeclaration, use conditions, lot CoACompliance file and incoming inspectionDeclaration covers grade and use; CoA matches lot

Swipe the table to see all columns →

5L Jerrycan Blow Molding Machine | Mold and Container Take-Off A representative 5l jerrycan blow molding machine | mold and container take-off clip. The machine, mold and configuration in your project may differ.

Two sheets at 0.955 g/cm3: a worked comparison

Here is an illustrative pair, not a grade recommendation. Grade A: 0.955 g/cm3, MI 0.25 g/10 min at 190 °C/2.16 kg, ESCR F50 with reagent and temperature stated. Grade B: 0.956 g/cm3, MI 0.45 g/10 min at the same condition, ESCR without test conditions. The density difference is inside normal lot tolerance; the MI difference is real; the ESCR comparison is not yet usable.

On an ES-5LS making a 5 L bottle, Grade B's higher MI should flow more easily, while Grade A's lower MI should give a more stable parison. On an ES-10LS, the longer parison favours Grade A's melt strength. These are expected directions, not measured results: run both grades on the same mold and compare wall thickness, drop and measured cycle.

Record the extruder profile, die gap, parison programmer settings, blow pressure and cooling for each grade; otherwise the comparison mixes resin with machine settings. Keep a lot sample and CoA for each grade, and repeat the wall check after a few hours.

Output arithmetic is separate: cavities x good parts per cavity x cycles per hour, where cycles per hour is 3,600 divided by the measured cycle time. A faster-flowing grade may shorten extrusion, but cooling usually dominates.

What to send for a quotation

A quotation can only be as specific as the resin information behind it. Send the following, and mark anything still open.

  • Container drawing: volume, neck, handle, target wall and decoration.
  • Both datasheets: density with method and tolerance, MI with load and temperature, ESCR method and F50, shrinkage and food-contact declaration.
  • Lot CoA for the resin you will run.
  • Filling product and conditions: chemical, concentration, temperature, shelf life and stack height.
  • Target output, shift pattern, cavity count and regrind use.
  • Destination, voltage and control preference.

Send the files through thecontact page; if you are still comparing platforms, start with the0.1–16 L single-station range.

Source: E-SHION product data. Specifications are subject to change without notice; customization is available.

This guide is written for production and procurement decisions. It uses published figures where available and avoids unverified performance claims.